Differential Scanning Calorimeter
1,520.00৳
⛟ Stock products delivery time 1-3 working days. 🔥
✈ Out-of-stock products delivery time 10-20 working days. 🚀
☎️ Contact Us for any inquiry
Product introduction:
The differential scanning calorimeter is a touch screen type, which can perform glass transition temperature test, phase transition test, melting and thermal enthalpy test, thermal stability test, and oxidation induction period test.
Comply with the following standards:
GB/T 19466.2–2004/ISO 11357-2:1999 Part 2: Determination of glass transition temperature
GB/T 19466.3–2004/ISO 11357-3:1999 Part 3: Determination of melting and crystallization temperature and enthalpy
GB/T 19466.6-2009/ISO 11357-3:1999 Part 6: Determination of oxidation induction time and oxidation induction temperature
Technical parameters:
1. Temperature range: room temperature ~ 500℃
2. Temperature resolution: 0.01℃
3. Temperature fluctuation: ±0.1℃
4. Temperature repeatability: ±0.1℃
5. Heating rate: 0.1~100℃/min
6. Constant temperature time: recommended <24h
7. Temperature control method: heating, constant temperature (fully automatic program control)
8.DSC range: 0~±600mW
9.DSC resolution: 0.01mW
10.DSC sensitivity: 0.01mW
11. Working power supply: AC220V/50Hz or customized
12. Atmosphere control gas: nitrogen, oxygen (instrument automatically switches)
13. Gas flow: 0-300mL/min
14. Gas pressure: 0.2MPa
15. Display mode: 15-inch LCD touch screen display
16. Data interface: standard USB interface
17. Parameter standard: equipped with standard substances (indium, tin, zinc), users can calibrate the temperature by themselves
Technical features:
1. Industrial-grade 15-inch touch screen, completely free from the constraints of computers.
2. Electronic flow meter, more accurate flow recording.
3. The touch interface is independent of the display, which is more flexible.
4. The unique sealing of the furnace can provide good experimental conditions.
5. Automatically switch the two-way atmosphere flow, with fast switching speed and short stabilization time. At the same time, add one protective gas input.
6. The software is simple and easy to operate.
Shipping Information
Out Of Dhaka: 1–3 working days for most locations within Bangladesh and cost only ৳120 TAKA.
Know more details.
Return Policy
You may return items purchased from Meter BD Shop within 7 days of receiving the product.
To be eligible for a return, the product must meet the following conditions:
1. Unused, 2. In the original packaging & 3. Proof of purchase.
Reviews
There are no reviews yet.